ORVAR SUPREME, ASSAB 8407, SKD61
Hardness after welding are tested in laboratory to be between 42 HRC to 48 HRC. The hardness are depending
on diameter of thread and parameters for welding.
Ø | 0.2 | 0.3 | 0.4 | 0.5 | 0.6 | 0.8 | 1.0 | 1.2 | 1.6 |
| | | | | | | | |